I remember reading an account by one of the sculptors of the period ( I forget who ) where he described the secrecy which shrouded the work of "le Patinateuers". ( forgive my mutilated spelling of the French language ). Apparently they even worked behind screens in their own studios to keep prying eyes out. I feel that many of the European methods were even more a matter of instinct than the oriental methods. As such written records of these processes are bound to be very much lacking.

Ford

 

Hi Ford and all others,

 

 

Yes, as you mentioned a lot of workshop secrets are vanished as the artists died. But one thing came to my mind when I compared very differend metalart-work from differend periods. The beauty of the patina or other layers on the metal depends more on the quality of the metals surface than the chemicals which are applied to it. :blink:

 

Here are some examples:

 

Giambolognia - Mercure

 

In the Renaissance some sculptors had painted their castings with organic lacquer and trusting on natural aging of the metal.

This painting concept was revitalized later in the Art Deco. Artists were again using laquer on polished metal.

 

Ferdinand Preiss

 

Nowadays a lot of founderys do not work on the metal to such an extend. :(

 

Here is some eye-candy from Japan. Traditional Style. :D

 

Chokichi Suzuki - Falcon

 

best regards

Karl

Link to comment
Share on other sites

  • Replies 89
  • Created
  • Last Reply
link to metal higo inaly

 

http://www.kougei.or.jp/english/crafts/0813/f0813.html

 

Remo

 

Hi Ford, I am using the recipe you have provided for my fittings. Thanks for that. I let a friend using the solution first (test run before I do mine). it worked realy well. He boiled them in tea and it looks great. The fittings were mild steel and had bronze inlay in them, same as the ones I'm doing.

 

One question though, I have noticed that the fittings have after a few days developed a sooty black coating on them that rubs off onto your hand, the fittings stay black but the soot is no good for keeping your hands clean. These are sword fittings already attached to the blade. I know he polished the fittings after boiling to bring out the inlay and they seamed fine at the time. I'm not sure how long he boiled them for though. I noticed in the Higo tutorial that they boil them for 30mins. I also see that the heat the fittings after until white some appears, I know he did'nt do that.

 

Has this happened to you, and will it disapear once cleaned again?

Any input on this slight problem would be great.

 

Regards Glen.

Link to comment
Share on other sites

This is an adjusted reciepe, based on a traditional Japanese rusting solution.

 

Vinegar 250 ml

Water 125 ml

Salt 5 grams

Copper Sulphate 1.5 grams

and 5 grams of liver of sulphur. ( Pottasium polysulphide ) or similar Jewellers silver "oxidising" solution.

 

Mix all the ingredients together and wipe onto the iron or steel just to wet the surface. Suspend the piece, I use a bent piece of wire as a simple hook, and allow to dry, Repeat twice a day, scrubbing any loose rust off when it appears. Use a stiff nylon brush or toothbrush. You can also periodically scrub the metal with crumpled up, wet newspaper. This process can take a week or more but can yield a very convincing colour for tsuba. Once you are satisfied with the depth of colour you can finish as described in some of the previous posts. The important thing is not to allow the rust to develop a crust, you want a thin layer of oxides ( and other compounds ) that doesn't encrust the surface, but enhances it.

 

good luck, Ford

 

p.s. Remo, I am now going to get those images of the chisels done. :blink:

 

Woops, sorry Ford and Remo,

 

My reply above this one was directed at this Post, but it relates to Both posts anyway.

Refer to above about Black soot after patination of steel.

 

Regards Glen........... Sorry

Link to comment
Share on other sites

Guest ford hallam

Hi Glen,

 

firstly let me apologise for not having welcomed you to our rapidly growing band of metal bashers earlier. I'm sure you'll have fun here. :D

 

I'm pleased the evil mix worked for you. I'd suggest that if there is any sort of residue still forming on the steel then the rust hasn't been neutralised effectively or some moisture has remained trapped in the steel. Once you have the sort of covering you want, and here it is important that you don't end up with a crust of rust but a very thin surface layer, you could try boiling the piece in a solution of sodium bicarbonate to neutralize the acid. Then proceed to boiling in tea or logwood chips ( another source of tannin). Before you apply the final wax coating you need to heat the steel until you have driven out any moisture. Do this gently and slowly and only for as long as moisture forms on the surface. Blot the water off with kitchen tissue or something similar. While to steel is still hot apply your wax. I use renaissance wax because it's so hard. Once the steel has cooled enough to allow you to handle it you can begin to softly work up a gloss, again using clean kitchen tissue.

 

 

The secret, if there is such a thing, to working up a good patina on steel is exactly that..."working it up". I tend to apply a number of overlapping processes to create depth and in the right light, subtle tonal variations. I've said it before, it's a bit like cooking :blink:

 

I hope this is of some use. If not, get back to me....there are other "tricks" but I'd rather not get too complicated, yet!

 

regards, Ford

Link to comment
Share on other sites

Thanks Ford for your help, can I ask one more question of you. Or of anyone else out there.................................

 

I have been applying the solution daily (dipping the fittings in actually and brushing off excess liquid). I wiped the fittings down after a couple of days with acetone and a rag, which removed quite a bit of rust and some fress areas of steel re-appeared.

 

After another coat and a day, there is some nice light brown surface rust over all areas, which I brushed the surface off with a tooth brush and have reaplied the solution. I noticed when brushing that there are nice orange/brown surface rust areas but there are deap dark areas in patches as well.

 

The question is, will these areas all darken up well and blend in together in the green tee in a couple of days time, or should I be aiming for one or the other effect. Ie Dark almost black areas or a nice light rust all over?

 

HELP!!!!! Regards Glen.

Link to comment
Share on other sites

Guest ford hallam

G'day :blink: , Glen,

 

the different colours you may be seeing are just the different stages the rust is going through. It will all blend in eventually. If you consider the mix you are applying you will see that there are a number of different compounds being formed. Some are acting on the steel while some are acting on the rust itself, hence the older rust being darker. All we're trying to do is simulate what happens naturally, and over a much longer time, to steel which is exposed to the elements. You may find yourself becoming a connoisseur of manhole covers :D , now there are excellent examples of what we want. Another good example would be old iron railings (out doors ) which have been handled daily for years. If you try to imagine how that glossy, thin, yet still tough, patina developed then you will have a better idea as to what it is you are trying to achieve. The most convincing results I've achieved have taken about 6 weeks and they are also by far the most durable.

 

You could also try just very lightly dampening the metal surface rather than drenching it and then wiping off excess. If you find that there are patches that seem to be resisting any rust development you can try "opening the surface" with a very light and quick swab, locally, of hydrochloric acid. Sometimes the surface is burnished a bit in the final polish and this tends to seal the metal a little. The quick etching action of the acid may be enough to create a more receptive surface. And I really do mean quick, the moment the metal has gone grey, rinse it off in water. That should be enough.

 

you'll get there :(

cheers, Ford

Link to comment
Share on other sites

Guest ford hallam

btw, that nice light orange brown is active rust :blink: , not desirable as a final finish at all. There are mid brown finishes ( I'd call then "russet iron") but that's a different thing and they are not all that wear resistant. They are also notoriously unstable in the wrong conditions.

Link to comment
Share on other sites

Hi Phil, Karl, Ford and welcome to the path to Glen

 

Phil and Karl, sorry I have been unable to thank you both sooner for your tips on patination, computer was sick for a couple of days :D kept losing my connection, but it's fine now :blink:.

 

Karl, I really like the Berlin iron braclet, very much like a cameo but made of iron.

 

Phil, I am a little reluctant to try out chemicals that I am not sure about, more so heating them etc, I have looked over your previous thread (#4) and have been searching the web for concoctions that have the simplest of solutions (i.e. chemicals).

 

I have found one simple solution on Sword Forum International, the post is by Brian VanSpeybroeck the link is http://forums.swordforum.com/showthread.ph...ght=black+tsuba.

 

I was wondering if yourself or Ford have tried this method and if the results were as expected.

Link to comment
Share on other sites

Hi Phil, Karl, Ford and welcome to the path to Glen

 

Phil and Karl, sorry I have been unable to thank you both sooner for your tips on patination, computer was sick for a couple of days :D kept losing my connection, but it's fine now :blink:.

 

Karl, I really like the Berlin iron braclet, very much like a cameo but made of iron.

 

Phil, I am a little reluctant to try out chemicals that I am not sure about, more so heating them etc, I have looked over your previous thread (#4) and have been searching the web for concoctions that have the simplest of solutions (i.e. chemicals).

 

I have found one simple solution on Sword Forum International, the post is by Brian VanSpeybroeck the link is http://forums.swordforum.com/showthread.ph...ght=black+tsuba.

 

I was wondering if yourself or Ford have tried this method and if the results were as expected.

 

Mike,

 

The concoction mentioned by Brian on SwordForum is the reason this thread was started - I tried it, and had success on some items (high carbon steel), and then had a failure (mild steel). The very first posting on page one of this thread (Rusting Question) describes the problem. The other recipes described are alternatives to the hydrogen peroxide/salt/vinegar.

Link to comment
Share on other sites

Hi Mike, Glen and all.

 

Glen, please pardon my manners, and welcome to the forum!!

 

The recipies and techniques in the attached link seem rather complicated, but I have tried variations on the heated version. There is a commerciallly prepared variation on the hot solution mentioned that I have used, and I have used the cold blue solution mentioned. Both can be useful for a quick patination of small parts like pins or screw heads, but the results produced over large surfaces are less than desirable.

 

I know a couple of gunsmiths who use cold blue, and let it sit for a while longer than specified before washing, which can produce more of a rusting effect, rather than bluing, but this too is unpredictable.

 

The solution that I mentioned and use requires no heating in either preparation or application, and is the same as used by military armourers and gunsmiths to brown or blacken iron and steel since the mid ninteenth century. A humidity tent is useful though, for any patination solution.

 

There are many ways to achieve the effect you are looking for. Ford's comments about building a good patina are dead on, regardless of the prefered solution. Unfortunately, there are no short cuts. A good patina can take many days to apply. Also, Ford's cautions about the red rust can not be understated. This can happen whenever any clorides (table salt, hydrochloric acid, etc) are used in an acidic solution. The piece must be thoroughly neutralized with either bicarbonate of soda, or sodium hydroxide (my preference, as there is no fooling around) boiling in either plain water or tea if you prefer will help afterward, and also darken the piece.

 

Interestingly, there was a study done at the Canadian Conservation Instititute a few years ago regarding coatings for ferrous metals, which involved exposing coated sand-blasted mild steel plates to the elements, in various locations, and those coated with just tannic acid (labratory grade) fared worse that the plain mild steel. Tannic acid coatings need to be quite heavy to have any effect, and must be backed up with a secondary coating. Unfortunately, the levels of tannin required to have any effect usually turn the piece a sort of purplish black/brown.

 

Phil

Link to comment
Share on other sites

Thanks Mike and Phil,

 

Phil, I think thats where it went wrong with my friends pieces, did'nt do the Bicarb part, just cleaned up and boiled in tea. Bugger, he's not gunna be happy as the pieces are still forming a black powder. trouble is the kashira is already mounted to the handle with the wrapping. all the rest can be re-done I guess.

 

Thank to all you Guys, Its been a real leaning experience. I'll see how I go. The fittings are all starting to darken up ok now. I'll give them a nother couple of days or so.

 

Cheers Glen.

Link to comment
Share on other sites

Hi Glen

 

Welcome to the path, Just had a quick look around your site, very impressed :blink:

 

Just a quick question, what is the katana kake in your displays made of (type of wood)?

 

Enjoy you time here

 

Regards

 

Mike Mc

 

Cheers for the kind words Mike,

 

The Katana kake were designed for small tanto and hunting knives to go on at a knife show. I bought 2 1" thick burl slabs from a wood turning shop in Croydon (Melbourne) and used the outer edges as the facing sections to add character. Then just cleared then with automotive acrylic laquer.

 

Regards Glen.

Link to comment
Share on other sites

Guest ford hallam

Hi Glen,

 

nah! we're always happy to help...where we can, and we like pictures :) .

 

not sure if you read this bit I posted earlier regarding those resistant areas; so just in case you missed it, here it is again :D

 

If you find that there are patches that seem to be resisting any rust development you can try "opening the surface" with a very light and quick swab, locally, of hydrochloric acid. Sometimes the surface is burnished a bit in the final polish and this tends to seal the metal a little. The quick etching action of the acid may be enough to create a more receptive surface. And I really do mean quick, the moment the metal has gone grey, rinse it off in water. That should be enough.

 

The rust that is developing is looking good though.

 

cheers, Ford :( (it's National Womans day here, so I've got to make my own lunch now!:blink: )

Link to comment
Share on other sites

Thanks Ford,

 

I did read that .......... Thanks. Just gotta work out where do get the stuff in the mean time. Don't know if chemists sell it? or is it available at the supermarket? I'm glad you think the rust is looking good, That's a sigh of relief.

 

Cheers Glen.

 

P.S. Do you do much in Japanese fittings? What I have found on the forum of your work is beutiful.

Link to comment
Share on other sites

Hi Tom

 

Thanks for the input, I didn't know that the Brian VanSpeybroeck recipe had been a subject here, or that it kicked off this thread, nice to know that so many are aiming for the same target, with mixed results, It is these results and failures that give the novice i.e. Me :blink: a chance to see tried and tested methods as done by others, and to spur the novice on to try their hand at these methods.

 

Thank you for your help and advice Tom.

 

Hi Phil

 

I must admit that I am a little timid with chemicals, as I have no background at all in this field, BUT, I am now willing to take the first step in using some of the recipe's put forward here by so many talented people.

 

I have had very little sucess in the natural patination (air rusting) that I tried, just tiny little pits of rust here and there, so I gave the 2 pieces to a friend who wants to try the cold bluing/browning methods.

 

I have had some sucess with the hydrogen peroxide, salt and vinegar solution over the past 2 days on a test piece of mild steel, I too had the problem where area's showed no reaction, So, using the methods outlined by Ford to "open the surface" where the steel resists rusting, I am glad to say that this worked and helped to even the coating of rust very well 'Thanks Ford'.

 

Thank you Phil for your valuable help.

 

I will upload some pictures when I work out how to post them here to show the progress to date.

 

All help and advice has been inwardly digested and set me on the road to new discoveries.

 

Thank you all

 

Mike Mc

Link to comment
Share on other sites

Guest ford hallam

Hi Glen,

 

you could try swimming pool maintenance suppliers. Hydrochloric ( or Muriatic acid ) is what we use here in South Africa, I assume you would use similar pool chemicals in Australia.

 

Thanks for the kind comment on my work :(, glad you liked what you've seen. I'll have quite a lot of new stuff to show in a little while. Some more tutorials too.

I don't do that many fittings really, nowadays perhaps one tsuba a year, for the NBTHK competition in Japan. I've been making kagamibuta for the last year but am also developing other, more contemporary, formats for my metalwork. There isn't much demand for the sort of traditional work you may be thinking of so it is important to develop alternative markets......or starve :blink:

 

Hi Mike, glad to hear my little tip helped. This sort of patination process is very variable but consistent results can be achieved with a bit of trial and error. We'll try and keep the error part to a minimum though. :D

 

keep at it fellas, Cheers, Ford

Link to comment
Share on other sites

Hi All

 

Just looked at how to upload images (posted by Janel), here is the test piece tsuba using the hydrogen peroxide, salt and vinegar method.

 

post-1602-1186662686.jpg

 

The plate has many more applications of the hydrogen peroxide, salt and vinegar solution and carding before it is finished, when I am happy with the results, I will use this practice piece as the learning curve on the actual tsuba that I am working on at the moment.

 

Thanks again all

 

 

Mike Mc

Link to comment
Share on other sites

Aloha

 

All this discussion of controlled iron oxidation and seeing Mike's tsuba (hello Mike). has me wondering. In the case of copper alloys and other non-ferrous metals inlaid in iron, how do you apply the different patina solutions to something like tsuba? That is to say the solutions mentioned here are quite different from rokusho and hiidoro. Which comes first? How would you protect the first patina from the second solution? I suppose these are questions for Ford or Patrick.

I recently received Lethal Elegance by Joe Earle. It raises many questions.

 

KC

Link to comment
Share on other sites

Guest ford hallam

Aloha Karl

 

now you are asking a serious question. If you really want the answer you must pledge either your first born or your soul. ;)

....OK perhaps it's not that complicated :rolleyes:

 

Do the rust based ground first then mask out the iron/steel ( very carefully) black nail varnish works well...and happens to suit me :blush:

 

The rokusho solution is then applied as a paste, it's somewhat different to the usual aqueous solution, I'll post the specific mix tomorrow. Again this is a slow process, 5 to 10 days usually.

Link to comment
Share on other sites